UJI FASTENING PADA KAYU KOMPOSIT SERAT PANDAN WANGI DAN LIMBAH KAYU DENGAN RESIN POLYESTER

Authors : Emmy Dyah Sulistyowati; Insan Andrian; Nasmi Herlina Sari; S. Sinarep; Pandri Pandiatmi
article cite 0 Year 2015
source: Dinamika Teknik Mesin
Abstract

The purpose of this study was to obtain handling connection type in use as door panels, roofing sheets, walls and floors. Therefore, the tests performed are fastening test and abrasion test. The technique of making wood composite is using hand lay-up technique. Constituent material of board composite is using pandanwangifibers with length variationsare 15 mm, 20 mm, and 30 mm with volume fraction variations are 20% and 30%, and 5% Sengon tree saw-dust is used as the filler. The results showed that pre-drilling with fastener sizes # 6, # 8 and # 10 is 3.5 mm, 4 mm and 4,5mm. The distance between each fastener depends on the fastener head itself, ie fastener # 6, # 8, and # 10. Critical distance between the edge of the fastener has a significant effect on fiber length and volume fraction. The highest value is shown on 15 mm of the fiber length and 20% of volume fraction with the value 3.29 mm, and the lowest value is shown on 15 mm of the fiber length and 30% of volume fraction with the value 2.74 mm.


Concepts :
Geotechnical and construction materials studies
article cite 0 Year 2015 source Dinamika Teknik Mesin
SDGs
Sustainable cities and communities
Citations by Year
YearCount
2015 0